Unveiling the interface: The fantastic ways to observe tribological contacts

By Andras L. Korenyi-Both, Contributing Editor | TLT Tribology Fundamentals December 2026

While direct visual observation of a tribological contact is extremely difficult, some clever solutions have been developed by tribology's pioneers.


Foundational concepts of friction, lubrication and wear can be experimentally verified by running tests where we rub (in Greek tribō) two opposing surfaces together and then after one cycle or millions of cycles, or somewhere in between, we take the two opposing surfaces apart and "look" at them. By measuring the input load and the tangential friction load during rubbing we can monitor the coefficient of friction in real time, but monitoring and measuring interfacial phenomena in real time is very challenging. Luckily, challenging and impossible are not synonymous and in this article, we review some of the prolific and very elegant ways tribologists have successfully pulled the cover off of buried interfaces. The three temporal domains related to the pair of objects in a tribology experiment are prior to, during and finally after the experiment. As a quick side note, unfortunately with most failure analysis from machinery that have encountered a tribological issue, we are presented with surfaces often with millions of cycles and a late-stage set of wear scars, so very much in the later time domain often referred to as postmortem. When we look at these surfaces that have been rubbed against each other the action of friction, wear and lubrication (or lack of) has already happened. As such we must infer and often make an educated guess as to what transpired in the beginning and during the wear process because the worn surfaces analyzed postmortem only exhibit the cumulative wear process and, in many cases, this is an amalgam of many complex events.

Tribologists are intrigued by, maybe even obsessed with, surfaces, a natural outcome of being scholars of objects whose surfaces are in contact under relative motion. Unfortunately, direct visual observation of a tribological contact, known as in situ or in operando observation, is very difficult primarily due to the geometric nature of a moving contact. Even without geometric constraints the Observer Effect in quantum mechanics postulates that the process of observation changes the object of interest relative to its unobserved state. Despite this unfortunate quantum pitfall, we still need to observe objects to gain understanding. Empirically, on a larger macro scale, during the intimate contact of two opposing surfaces there is a geometry constraint where we can't exactly "peek in" to the real contact without disrupting the mechanism. Most observational methods can be used to investigate contact surfaces immediately before or after they have been rubbed together but the really rare and interesting methods are the ones that allow a glimpse into the contact in real time.

Experimentally, an extremely clever solution to the buried interface challenge was first reported from Cambridge University by Bowden and Tabor in the 1950s. These pioneers of modern tribology used translucent materials such as glass or quartz to slide against various materials coupled with an optical microscope to observe the evolution of wear.1 By sliding various metals such as steel, aluminum or copper across a flat rotating glass disk, Bowden and Tabor were able to observe several key tribological aspects of friction and wear. The first aspect was being able to visualize the relatively small real area of contact limited to surface asperities, the peaks of the metal surfaces, in contrast to the deceivingly large apparent area of contact. At higher rotational speeds, they witnessed hot spots as the small asperities started to glow from extreme frictional heating; these microscopic junctions were glowing red hot! If the metallic slider was relatively soft, they were also able to observe the onset of adhesive slider wear. This approach pioneered by Bowden and Tabor allows us to see the contact during sliding, so truly in operando, but one of the surfaces, the glass disk needed to be optically translucent. Seeing in the English language implies a vision process involving our own photon sensors, our eyes, it is by definition an optical event and a convenient way of seeing the contact. This is just one type of sensor to be considered, although very familiar to us, there are others that can help us better understand complex tribological interfaces.

We can dig into our physics toolbox and find other sensors or detectors specializing in regions in the electromagnetic spectrum other than visible light. If we stay with the concept of optical transparency for one of the components then we can excite the contact by passing energy through the translucent pair and observe what comes back and record it with a detector. This detector can be a human eye, photographic film or a modern digital Charge-Coupled Device (CCD) array. Not only did Bowden and Tabor pioneer a visual portal into the rubbing contact, they verified their observations with ingenious combinations of other sensors such as electrical contact resistance, thermal and even mechanical sensors. For using an electrical resistance signal, the nonconductive glass was replaced by a metallic contact and by measuring the changes in electrical resistance across the metal-to-metal (or metal-to-conductive substrate) junctions, they could calculate exactly how many microscopic asperity tips were touching at any given millisecond. The electrical resistance sensor readings fluctuated wildly during sliding, proving that microscopic junctions were constantly welding together and breaking apart, providing the first physical evidence of stick-slip motion. Often stick-slip results in an audible signal, a squeak, thus another sensor that can be used to monitor an interface is an acoustic sensor. During this same period Kaiser established that metals emit high-frequency acoustic waves when subjected to mechanical stress.2 Additionally, to measure the flash temperatures between two non-translucent surfaces, Bowden and Tabor used two sliding metals as thermocouple junctions as the two distinct elements of a thermocouple. As the asperities rubbed together and generated heat, the rubbing action produced a small, measurable thermoelectric voltage (electromotive force, or EMF) proportional to the interface temperature. This sensor setup provided proof that even if the bulk metal feels cool to the touch, the microscopic contact points routinely flash to temperatures exceeding 1,000°C in a fraction of a millisecond. This is a very important concept to realize as often well-meaning engineers are convinced that temperatures are low based on global part temperature data, but in reality, deep in the contact, temperatures on asperities are extremely high.

Inspired by the seminal work of Bowden and Tabor, Buckley in the 1970s at the NASA Lewis Research Center continued this work as a pioneer in space tribology.3 Another interesting outcome of the Bowden and Tabor experiments proved that ambient moisture changes how glass wears. Buckley took this to the next level by placing glass-and-metal sliding setups inside ultra-high vacuum chambers simulating outer space. He confirmed that in a vacuum, without any air or surface films to buffer the contact, materials like aluminum, iron and gold adhere to glass so violently that the surfaces quickly experience massive cold welding and transition entirely to glass sliding on itself. Buckley used the lessons learned from glass experiments to drive NASA's broader research for spacecraft bearings, seals and high-temperature engine coatings. He expanded upon Bowden and Tabor's macroscopic visual theories by integrating atomic-level surface science, analyzing how crystal orientation and atomic valence bonds dictate whether a material will wear down or resist friction.

Stepping forward to the late 1990s, Singer continued to refine this concept of transparent sliding interfaces. Bowden and Tabor treated wear as a matter of a "first body" (the slider) rubbing against a "second body" (the substrate). Singer proved that real friction and wear are also controlled by a "third body," the dynamic layer of trapped wear debris, sheared particles and chemical transfer films generated inside the sliding contact. To observe these third bodies in real time, Singer pressed transparent glass or sapphire hemispheres against thin film low friction coatings.4 Singer's technique synced a fast-sampling friction sensor with the exact physical coordinates of a reciprocating sliding path as observed through the translucent rider. By looking through the glass slider with high-speed video and mapping the friction locally in the wear track, Singer could point to a sudden spike in a graph and look at the video to see exactly what caused it; this could be a single speck of trapped debris or a local coating delamination. Taking this concept further Singer and his colleagues at the Naval Research Laboratory pointed a laser beam directly through the back of the transparent glass hemisphere right into the sliding contact zone while the test was running and then used a Raman spectrometer to see or read the laser reflection to determine the exact molecular chemistry at the interface as the slider rubbed against the substrate.5



In the late 2000s researchers at the Air Force Research Laboratory built an in situ micro-tribometer inside a focused ion beam vacuum chamber. By stopping the sliding test and immediately using ion beam deposition to weld the active sliding tip to the film under a heavy mechanical load, they extracted a cross-sectional transmission electron microscope (TEM) specimen precisely at the active contact point without tip/film separation. This completely eliminated postmortem structural relaxation artifacts during TEM analysis.6 Thus, Hu et al. pioneered yet another clever technique to look at a tribological contact and observe the true nature of the material surfaces without all the unintended artifacts that would be introduced with classic postmortem analysis. Because the tip and the worn material were welded together during the experiment, the subsequent high-resolution TEM (HRTEM) and energy-dispersive X-ray spectroscopy (EDS) analysis mapped the exact atomic-scale matching, mixing and crystal orientation at the true sliding interface. Their work utilized this setup to show exactly how complex transition metal dichalcogenide (TMD) alloy systems self-organize under shear. They verified how the atoms line up along their basal (002) planes under load to create an ultra-low friction interface, tracking how individual dopant elements like tungsten and selenium segregated or consolidated to prevent environmental degradation.

Recent work by Koly and colleagues highlighted a clever approach to in situ scuffing tribology by placing a tribometer into an X-ray beam line at the Advanced Photon Source facility at Argonne National Laboratory. A thin stationary disk, to maximize X-ray transparency, was run with a cross cylinder counterface geometry and friction data was collected at the same time as X-ray diffraction data was collected from the interface.7 This novel approach brought new light and understanding to scuffing mechanics.

Although not fully inclusive of all the clever and innovative ideas to discover tribological interfaces, this article highlights some critical ones. These innovations have not only led to new discoveries and insights for science and engineering but have continuously spurred the next iteration of successfully lifting the veil of buried tribological interfaces, allowing us to peek into contacts to further advance the field of tribology.

REFERENCES
1. Bowden, F. P. and Tabor, D. (1950), The friction and lubrication of solids (Part 1), Clarendon Press.
2. Kaiser, J. (1950), Untersuchungen über das Auftreten von Geräuschen beim Zugversuch (Investigations on the Occurrence of Noises in Tensile Tests), Ph.D. thesis, Technische Hochschule München (Technical University of Munich).
3. Buckley, D. H. (1974), "Friction behavior of glass and metals in contact with glass in various environments (NASA Technical Note D-7529)," National Aeronautics and Space Administration.
4. I. L. Singer (1998), "How third-body processes affect friction and wear," MRS Bulletin, 23 (6), pp. 37-40.
5. Singer, I. L., Dvorak, S. D., Wahl, K. J. and Scharf, T. W. (2003), "Role of third bodies in friction and wear of protective coating," Journal of Vacuum Science & Technology A: Vacuum, Surfaces, and Films, 21 (5), S232-S240.
6. Hu, J. J., Wheeler, R., Zabinski, J. S., Shade, P. A., Shiveley, A. and Voevodin, A. A. (2008), "Transmission Electron Microscopy Analysis of Mo–W–S–Se Film Sliding Contact Obtained by Using Focused Ion Beam Microscope and In Situ Microtribometer," Tribol. Lett. 32, 155-164.
7. Koly, F. A., Bhattacharjee, A., Murthy, N. et al. (2025), "Methods to observe tribological failures in self-mated steel contacts," Tribol Lett, 73, 35, https://doi.org/10.1007/s11249-025-01971-8.

Andras L. Korenyi-Both is Woodward Senior Technical Fellow Tribology at Woodward Inc. in Fort Collins, Colo. You can reach him at andy.korenyi-both@woodward.com.