Metals: A promising new fuel
By Don Smolenski, Contributing Editor | TLT Machinery December 2026
Iron is promising as a reusable fuel due to its cost, abundance and energy density, among other characteristics.


This comes out of nowhere!1 Metal ingots do not easily ignite. But they apparently will easily ignite when pulverized. Iron already powers rockets. Can it be a fuel here on Earth? Researchers are exploring the possibilities of iron and other metals as fuels on Earth. Burning pulverized iron, possibly in coal plant boilers that are being retrofitted, could provide free heat without the CO
2. But what about the byproducts of burning iron, for instance? Iron oxide is actually fairly simply recycled.
How about aluminum as a fuel? Aluminum could also be used as a fuel, but its combustion is hard to control, so would likely be too dangerous. Burning iron doesn't produce CO
2, so this is important. Iron is the second most abundant metal in the Earth's crust. It also is the cheapest metal and the cheapest on the market. It holds more energy than coal, diesel or gasoline. It's also easier and safer to transport. A lot of very promising characteristics!
Start-ups are exploring metals as a fuel on Earth because retrofitted coal plant boilers could be used. Burning pulverized iron, possibly in retrofitted coal plant boilers, could provide carbon-free heat: when iron burns to form iron oxide, the process is reversible. So there's potentially promising cheap fuel and also long-term energy storage. It is promising as a reusable fuel, promising cheap reusable fuel and long-term energy storage.
2 The challenge is to make it cost-competitive with natural gas and to build support for adoption.
So where are these researchers? Now a group of scientists and start-ups wants to burn iron powder for heat and electricity. The Metal Energy Hub
3 at the Technical University of Darmstadt (I actually have some contacts there!) plans to retrofit a shuttered coal power plant. Countries seek to cut emissions and wars disrupt fossil fuel supplies. These forward thinkers believe iron is the cheap, carbon-free fuel the world needs. "We title it 'the new iron age,'" says Marius Schmidt, managing director of the Metal Energy Hub.
REFERENCES
1.
https://cen.acs.org/articles/95/i27/s-fireworks-produces-those-colorful.html?sc=260805_news_eng_cennews_cen&elqE=18222&elqC=10527
2.
https://cen.acs.org/energy/iron-fuel-combustion-energy-heat/104/web/2026/08?sc=260805_news_eng_cennews_cen&elqE=18222&elqC=10527#container-ad7983826c
3.
https://metalenergyhub.de/
Don Smolenski is president of his own consultancy, Strategic Management of Oil, LLC, in St. Clair Shores, Mich. You can reach him at donald.smolenski@gmail.com.