Home > Events > Calendar of Events
Event Details
Filter By:  
View: SUMMARY   MONTH   WEEK   DAY   DETAILS   Display:

Previous Month
March 2014
  S M T W T F S
01
02 03 04 05 06 07 08
09 10 11 12 13 14 15
16 17 18 19 20 21 22
23 24 25 26 27 28 29
30 31
April 2014
  S M T W T F S
01 02 03 04 05
06 07 08 09 10 11 12
13 14 15 16 17 18 19
20 21 22 23 24 25 26
27 28 29 30
May 2014
  S M T W T F S
01 02 03
04 05 06 07 08 09 10
11 12 13 14 15 16 17
18 19 20 21 22 23 24
25 26 27 28 29 30 31
Next Month

Webinar: Guidelines for Selecting Additives to Use in Metalworking Fluids

Thursday, March 27, 2014

12:00 PM - 01:30 PM


Join us for this webinar, where Dr. Neil Canter will present on "Guidelines for Selecting Additives to Use in Metalworking Fluids."

Guidelines for Selecting Additives to Use in Metalworking Fluids

Instructor: Neil Canter, Chemical Solutions

Where: STLE University, live webinar event broadcast to your computer

When: Thursday, March 20, 2014 at 12-1:00 p.m., with optional Q&A from 1-1:30 p.m. Central Time

Cost: $39 for members, $59 for non-members

Abstract

Selection of metalworking fluid additives is quite challenging because formulators are faced with developing products that contain as many as 20 components drawn from 13 different component types. Besides using the right components at the proper treat rate to prepare a stable metalworking fluid, formulators must make sure that the product works well under a diverse range of difficult operating conditions and also must be in compliance with the health & safety guidelines of the end user and the region where the end user is located. Examples of additive classes to be reviewed are emulsifiers, extreme pressure additives and reserve alkalinity boosters (amines). Different options are available to the metalworking fluid formulator in all three categories. One consideration that will be addressed is how formulations should be modified to minimize concerns that may arise as the metalworking fluid industry must comply with the Global Harmonized Standard (GHS) by the end of May, 2015.

Presenter Biography

Neil Canter received his PhD in Chemistry from the University of Michigan in 1983 and his BS in Chemistry from Brown University in 1978. He has been working in the lubricant industry for over 25 years. Neil previously worked for Stepan Company and Mayco. Presently, Neil runs his own consulting company called Chemical Solutions. He specializes in commercial development, marketing, product development and regulatory support for the lubricant industry.

Neil is a member of American Chemical Society, Society of Automotive Engineers (SAE) and the Society of Tribologists and Lubrication Engineers (STLE). Neil is currently a Contributing Editor responsible for writing the monthly Tech Beat column in STLE’s TLT magazine. He is also a member of the STLE Education Committee and the Chairman of STLE’s Metalworking Fluid Steering Committee.

In addition to the Tech Beat column, Neil has covered many topics on MWFs, additives and GHS via articles, presentations at past STLE local section meetings, and instructing in our upcoming Annual Meeting education courses, MWF 125 and MWF 130.

Contact Us

Phone: (847) 825-5536

Email: Kara Sniegowski at ksniegowski@stle.org

Reminder: Computer speakers or headphones are needed to hear the audio.

Registration is now open. Log in to your account at www.stle.org, then click on the link below to get to the event listing. Once you arrive at the event listing, click "add to your products" to start the purchase process.

Register for this event.Click Here to register for this event.

 
©2008 STLE All rights reserved.