Keywords

Aluminum, Rolling Oil, Contaminants, Vacuum Distallation

Track

Non-Ferrous Metals III (Session 7D)

Aluminum Cold Mill Rolling Oil Distillation 

This presentation is mainly about using an effective and simple method of clarification or refining of the aluminum cold‐mill rolling oil. The method uses vacuum distillation for the used, contaminated or degraded rolling oil to extract the good base oil plus the additives for reuse in the rolling process, and discharge of the bottoms for use in heating applications.

Authors and Company/Institution

Mohammed Albedour, Filtertech Inc., Manlius, NY