Metallurgical Analysis, Unlubricated Friction, Galling, High Temperature Tribology

Track

Material Tribology IV (Session 7B)

Influence of Microstructural Evolution of Al-Si Coated Ultra-High Strength Steel on the Tribological Behaviour

In recent years, the usage of the hot stamping process has increased due to the high demands for production of ultra-high strength steels (UHSS). In particular, more studies are being carried out pertaining to the Al-Si coated UHSS to understand its behaviour during the forming process as well as the performance of the produced parts. The Al-Si coating is applied to the UHSS with the aim of reducing decarburisation and to avoid the formation of thick oxide scales on the work-piece during the heating stage.

Authors and Company/Institution

Leonardo Pelcastre, Jens Hardell and Braham Prakash, Division of Machine Elements, Lulea University of Technology, Lulea, Sweden