Home > Events > Calendar of Events
Event Details
Filter By:  
View: SUMMARY   MONTH   WEEK   DAY   DETAILS   Display:

Previous Month
December 2012
  S M T W T F S
01
02 03 04 05 06 07 08
09 10 11 12 13 14 15
16 17 18 19 20 21 22
23 24 25 26 27 28 29
30 31
January 2013
  S M T W T F S
01 02 03 04 05
06 07 08 09 10 11 12
13 14 15 16 17 18 19
20 21 22 23 24 25 26
27 28 29 30 31
February 2013
  S M T W T F S
01 02
03 04 05 06 07 08 09
10 11 12 13 14 15 16
17 18 19 20 21 22 23
24 25 26 27 28
Next Month

STLE Philadelphia Section Meeting

Thursday, September 20, 2012

01:30 PM - 06:00 PM


Join the STLE Philadelphia Section for their first education meeting for 2012-2013, where Jerry Byers will presentation on Corrosion Issues and Testing Methods and Dr. Fred Passman will present on Metalworking Fluid Hot Topics: Microbicides

Philadelphia Section
Education Meeting
September 20, 2012

Title:
Corrosion Issues and Test Methods
&
MWF Hot Topics: Microbicides

Presenter:
Jerry Byers, Cimcool Fluid Technology and STLE President
&
Dr. Fred Passman, BCA Inc.

Abstract:
Corrosion Issues and Test Methods
– The presentation will cover test methods used to evaluate the corrosion of metals. The focus will be on using a specific corrosion test method to examine each of five metals commonly used in industry. Presented by Jerry Byers

MWF Hot Topics: Microbicides – An update will be provided on regulatory issues involving the restriction of the use of formaldehyde-condensate microbicides by the US EPA. Included will be background on what has been proposed and the potential consequences for the US Metalworking Fluid Industry. Presented by Dr. Fred Passman

Meeting Location
Brittingham’s Irish Pub and Restaurant
640 E. Germantown Pike
Lafayette Hill, PA 19444
(610)828-7351
http://www.brittinghams.com/   

Schedule
September 20, 2012
1:30 p.m. Presentations
5:00 p.m. Dinner

For more information or to make your reservation please contact Bill Wambaugh at bwambach@comcast.net or Mary Moon at m.moon@fluitec.com, (201)268-4359

For more information about the Philadelphia section please visit their website. Click the link below: http://www.philadelphia-stle.org/  

 
©2008 STLE All rights reserved.