Home > Events > Calendar of Events
Event Details
Filter By:  
View: SUMMARY   MONTH   WEEK   DAY   DETAILS   Display:

Previous Month
May 2014
  S M T W T F S
01 02 03
04 05 06 07 08 09 10
11 12 13 14 15 16 17
18 19 20 21 22 23 24
25 26 27 28 29 30 31
June 2014
  S M T W T F S
01 02 03 04 05 06 07
08 09 10 11 12 13 14
15 16 17 18 19 20 21
22 23 24 25 26 27 28
29 30
July 2014
  S M T W T F S
01 02 03 04 05
06 07 08 09 10 11 12
13 14 15 16 17 18 19
20 21 22 23 24 25 26
27 28 29 30 31
Next Month

Webinar: Wire Rope and Chains-Wear Mechanisms & Means of Lubrication and Maintenance

Wednesday, May 14, 2014

12:00 PM - 01:30 PM


Join us as Paul Conley from SKF walks us through lubrication practices for wire ropes and chains.

Wire Ropes & Chains: Wear Mechanisms and Means of Lubrication & Maintenance

Instructor: Paul Conley, Chief Engineer, Lubrication Business Unit, SKF

Where: STLE University, live webinar event broadcast to your computer

When: Wednesday, May 14, 2014 at 12-1:00 p.m., with optional Q&A from 1-1:30 p.m. Central Time.

Cost: $39 for members, $59 for non-members

Abstract

Wire ropes and chains are important mechanisms for transmitting tensile loads where flexibility is needed. As with any metal to metal contact system where relative motion exists, wear is an important consideration. This presentation will discuss the geometry of wire ropes and chains, wear tendencies and methods of lubrication and maintenance.

Presenter Biography

Paul Conley has been chief engineer at SKF/ Lincoln Industrial since 1997. Paul is a reqistered profession engineering in the state of Missouri and holds BS and MS in Engineering  from St. Louis University and University of Missouri Science and Technology respectively.

Paul has published several papers in the field of lubrication. Holds 15 patents with 12 pending. Paul is a contributing author in the STLE Handbook of Lubrication and Tribology. Paul is a  member of STLE, NLGI, ASTM and AISI.

Contact Us

Phone: (847) 825-5536

Email: Kara Sniegowski at ksniegowski@stle.org

Reminder: Computer speakers or headphones are needed to hear the audio.

Registration will open soon. Please ensure you're logged in at www.stle.org first, then click on the link below. Once you arrive at the event listing, click "add to your products" to start the purchase process.

Register for this event.Click Here to register for this event.

 
©2008 STLE All rights reserved.