Home > Events > Calendar of Events
Event Details
Filter By:  
View: SUMMARY   MONTH   WEEK   DAY   DETAILS   Display:

Previous Month
March 2013
  S M T W T F S
01 02
03 04 05 06 07 08 09
10 11 12 13 14 15 16
17 18 19 20 21 22 23
24 25 26 27 28 29 30
31
April 2013
  S M T W T F S
01 02 03 04 05 06
07 08 09 10 11 12 13
14 15 16 17 18 19 20
21 22 23 24 25 26 27
28 29 30
May 2013
  S M T W T F S
01 02 03 04
05 06 07 08 09 10 11
12 13 14 15 16 17 18
19 20 21 22 23 24 25
26 27 28 29 30 31
Next Month

STLE Central Illinois Section Meeting

Wednesday, January 09, 2013

05:30 PM - 08:00 PM


Join the Central Illinois section for their first meeting of 2013, where Kevin Austin will talk about Golf Balls and Bearing – how dimples can dramatically affect the lambda factor.

Central Illinois Section Meeting
Golf Balls and Bearings
January 09, 2013

Golf Balls and Bearings: How dimples can dramatically affect the lambda factor
Presenter: Kevin Austin

Abstract:
With the viscosity of the oils being used in transmission and differentials becoming lower, oil film parameter lambda can fall below 0.5 (VG10 oil used). In order to handle such increasingly severe lubrication conditions, NTN has developed Micro HL (high-lubrication) tapered roller bearings.

NTN’s unique micro-pitting surface finish increases bearing life in applications with insufficient lubrication. Based on the theory that oil film formation in bearing contact areas can be improved by changing the character and direction of the components’ surface finishes, the distinguishing micro-pots are able to effectively capture and channel oil to where it’s needed

Meeting Location
Barrack’s Cater Inn
1224 W. Pioneer Parkway
Peoria, IL 61615
(309)692-3990

Schedule
5:30-6:30 p.m. Dinner and Networking
6:30-7:30 p.m. Presentation
7:30-8:00 p.m. Questions/Discussion

Fees
$25.00 per person
$15.00 for students and retired members

To make reservations, contact Mike Davis at (217)855-8828 or email michael.davis253@frontier.com.

 
©2008 STLE All rights reserved.