N-ALKYLALKANOLAMINES AND N-ALKYLALKANOLAMINE DERIVATIVES FOR METALWORKING: e.g. TERTIARY N-ALKYLALKANOLAMINES-N-OXIDES

This talk will focus on tertiary alkanolamine and derivatives like the alkanolamine-N-oxides as useful heat activated boundary lubricants, antioxidants and persistent long term fluid stabilizing additives. The utility of the N-alkylalkanoalmines and certain alkanolamine derivatives as metalworking fluid additives will be illustrated.

AUTHORS

Michael D. Gernon and Guy Verdino, Taminco, Pace, FL